Dec 02, 2024 Atstāj ziņu

DN15

1/2

21.30

3.25

1.45

DN20

3/4

26.80

3.50

2.01

DN25

1

33.50

4.00

2.91

DN32

5/4

42.30

4.00

3.78

DN40

3/2

48.0

4.25

4.58

DN50

2

60.00

4.50

6.15

DN65

5/2

75.5

4.50

7.88

DN80

3

88.5

4.75

9.81

DN100

4

114.00

5.00

13.44

DN125

5

140.00

5.50

18.24

DN150

6

165.00

5.50

21.63

DN219

8

219

7

36.6

DN273

10

273

7

45.92

DN325

12

325

8

62.54

DN377

14

377

8

72.80

Nosūtīt pieprasījumu

whatsapp

Telefons

E-pasts

Izmeklēšana