SA214 ERW Carbon Steel Heat Exchanger Tube
Specification A214 covers minimum wall thickness, resistance welded carbon steel pipe used in heat exchangers, condensers and similar heat transfer equipment.
Nosūtīt pieprasījumu
Tērzēšana tūlīt
Produkta ievads
Tube sizes supplied to this specification are typically up to and including 3 in. [76.2 mm] outside diameter. Other sizes of tubing are available, but they must comply with all other requirements of this specification.
ASTM A214 Heat Exchanger Pipe Specification
| ASTM A214 | |
| 4 to 219mm W. T.: 0.5 to 20mm | |
| 10 Swg., 12 Swg., 14 Swg., 16 Swg., 18 Swg., 20 Swg. | |
| SCH5, SCH10, SCH10S, SCH20, SCH30, SCH40, SCH40S, STD, SCH80, XS, SCH60, SCH80, SCH120, SCH140, SCH160, XXS | |
| BA (Bright & Annealed), Polished, AP (Annealed & Pickled), MF, NO.1, Mirror finish, 2B, BA, NO.4, HL, 8K, etc | |
| SA214 Tubing are available in form of Round, Square, Hollow, Rectangular, Hydraulic, Coiled, Straight Boiler Tube, "U" Shape, Pan Cake Coils etc. | |
| EFW / Seamless / DOM / ERW/ Fabricated / Welded / CDW / CEW ASME ASTM A214 Carbon Steel Tube | |
A 214 Condenser Tubes Chemical Composition
| A/SA 214 | |
| C | 0.18 max. |
| 0.27 - 0.63 | |
| P | 0.035 max |
| S | 0.035 max |
SA 214 Carbon Steel Heat Exchanger Tubing Mechanical Properties
| A/SA 214 | |
| 47[325] | |
| 26[180] | |
| Greater than or equal to 35% | |
| Less than or equal to 72 HRB |
A214 ERW Tubing